Hempalin Undercoat 42460
Alkyd undercoat · INTL · manufacturer-sourced
How long does Hempel Hempalin Undercoat 42460 take to dry?
Short answer
Coat-by-coat plan
Touch-dry, recoat and washable are three different dates
- Cut in and roll the Alkyd undercoat in even coats
- Wait for the recoat time, not touch-dry
- Hold off scrubbing until the cure time
This product’s stated stages Quoted at 68°F
- Safe to touch4 hours
Worth noticing: The manufacturer states only one timing here (safe to touch, 4 hours); nothing else is inferred.
Common mistake: Closing the door or hanging pictures once the wall feels dry, long before the film has hardened.
Plan the next coat
Your countdown
Stated times
- Safe to touch4 hours
From Hempel data sheet · checked 2026-10-25. Anything not listed isn’t stated by the manufacturer.
Manufacturer website: hempel.com
Conditions & fine print
- Stated conditions: 68°F (20°C)
- Dry and recoat times change with temperature, humidity and film build. Follow the current data sheet and label.
- Apply at 41°F or above
- Region INTL. Formulas can differ between countries; check your container.
- Safe to touch: At 20°C and 40 microns dry.
- Entered from the cited manufacturer documentation. Check the current label for the exact formula and region. Report outdated information
- Actual results depend on preparation, thickness, ventilation, temperature, humidity, mixing and substrate.
Confirm this is your product
Closely named formulas, colors and regional versions can use different times. Match these details to your container before starting a countdown.
- Exact listing
- Hempel Hempalin Undercoat 42460
- Variant
- Alkyd undercoat
- Region
- INTL
- Listed use
- wood, steel, interior alkyd system
- Timed stages recorded
- touch
- Source checked
- 2026-10-25
Documentation: Technical data sheet · Product data sheet 42460
Condition attached to the stated time: At 20°C and 40 microns dry.
About this product
An alkyd undercoat, touch dry in 4 hours at 20°C. The sheet gives no overcoating interval and says Hempel's specification governs.
Using this specific product
Hempel Hempalin Undercoat 42460 is listed here as the Alkyd undercoat version for wood, steel, and interior alkyd system. For painting, the useful question is not simply whether the surface looks finished—it is whether the exact next-action milestone shown above has been reached.
Before you start
- Confirm the package says Alkyd undercoat; related versions can use different timing.
- For wood, steel, and interior alkyd system, pay particular attention to surface preparation, coat thickness and ventilation.
- At 20°C and 40 microns dry.
How to check readiness
Test an inconspicuous area for firmness and blocking before normal use. Touch only a hidden edge first; a dry surface can conceal a soft layer underneath.
Avoid this mistake
Recoating too early can trap solvent or water; waiting much longer may require scuffing under the label directions.
Compare with similar products
- Compare with Crown GP Matt Finish BlackTouch-dry: 4 h there, 4 h here.
- Compare with Krylon Farm & Implement Protective PaintTouch-dry: 4 h there, 4 h here.
Questions
How long does this product take to dry?
Hempel states: The sheet gives touch dry in 4 hours. Conditions: At 20°C and 40 microns dry.. These are the manufacturer’s stated times, not a guarantee.
How long does Hempalin Undercoat take to touch dry?
The sheet gives 4 hours at 20°C and 40 microns dry.
What affects how long this product takes to dry or cure?
Dry and recoat times change with temperature, humidity and film build. Follow the current data sheet and label. Follow the product label for your conditions.
Similar products
- Dulux X-Pert Interior Latex Primer/Sealer 11000Interior latex primer (Canada) · Paint, primer & patch · CARecoat 2–4 hours
- Dulux Weatherguard Exterior Primer 1535100% acrylic exterior primer (Canada) · Paint, primer & patch · CARecoat 1 hour
- Asian Paints Apcolite Premium EmulsionInterior acrylic emulsion · Paint, primer & patch · INTLTouch 30 minutes