Manufacturer-stated times

ProductManufacturer-stated minimumCondition/source
Interlux Micron 66 Antifouling
Ablative bottom paint
12 hoursSubstrate temperature
AquaBond SR-3000 Structural Repair Compound
Pool and spa epoxy
1 daysAt manufacturer-stated conditions; temperature, humidity and film thickness can change drying time.
AquaBond UW-5000 Underwater Repair Compound
Two-part epoxy
1 daysAt manufacturer-stated conditions; temperature, humidity and film thickness can change drying time.
Atlas Minerals Pool Putty
Underwater epoxy putty
1 daysAt manufacturer-stated conditions; temperature, humidity and film thickness can change drying time.
Pool Patch Pool Deck Repair Kit
Cement repair
2 daysAt manufacturer-stated conditions; temperature, humidity and film thickness can change drying time.
Ramuc DS Acrylic Pool Paint
Water-based acrylic
3 daysAt manufacturer-stated conditions; temperature, humidity and film thickness can change drying time.
Olympic Poxolon 2 Epoxy Pool Coating
Two-part epoxy
5 daysAt manufacturer-stated conditions; temperature, humidity and film thickness can change drying time.
Olympic Zeron Epoxy Pool Coating
High-build epoxy
5 daysAt manufacturer-stated conditions; temperature, humidity and film thickness can change drying time.
Ramuc Hi Build Epoxy Pool Paint
Two-part epoxy
5 daysAt manufacturer-stated conditions; temperature, humidity and film thickness can change drying time.
INSL-X Epoxy Pool Paint
White
7 daysAt manufacturer-stated conditions; temperature, humidity and film thickness can change drying time.
INSL-X Waterborne Pool Paint
Ocean blue
7 daysAt manufacturer-stated conditions; temperature, humidity and film thickness can change drying time.
QUIKRETE Advanced Polymer Non-Sag Sealant
Gray / tan
7 daysTemporary immersion
QUIKRETE Advanced Polymer Self-Leveling Sealant
Gray
7 daysTemporary immersion
Ramuc Type A-2 Premium Rubber Pool Paint
Rubber-based
7 daysAt manufacturer-stated conditions; temperature, humidity and film thickness can change drying time.
Sider-Crete Roll-On Pool Plaster
Cementitious coating
7 daysAt manufacturer-stated conditions; temperature, humidity and film thickness can change drying time.
TEC (H.B. Fuller) AccuColor Plus Grout (450)
All colors
7 daysSee product page
LATICRETE SPECTRALOCK PRO Premium Grout
Epoxy (all colors)
10 daysAt 70°F
Custom Building Products CEG-Lite 100% Solids Commercial Epoxy Grout
All colors
14 daysSee product page
Custom Building Products Polyblend Plus Sanded Grout
All colors (cement-based)
14 daysSee product page
Custom Building Products ProLite Premium Large Format Tile Mortar
Gray / white (TDS-114)
14 daysWater at 70°F (21°C).
Custom Building Products ProLite RS Premium Rapid Setting Large Format Tile Mortar
Gray / white
14 daysWater at 70°F (21°C).
Custom Building Products VersaBond Lite Professional Large and Heavy Tile Mortar
Gray / white (TDS-451)
14 daysWater at 70°F (21°C).
LATICRETE 254 PLATINUM Plus
Polymer-fortified thin-set mortar
14 daysWater at 70°F (21°C).
LATICRETE LATAPOXY 300 Adhesive
Epoxy tile adhesive
14 daysWater at 70°F (21°C).
LATICRETE PERMACOLOR Grout
All colors
14 days70°F and 50% RH
LATICRETE SPECTRALOCK 1 Pre-Mixed Grout
Translucent (DS-65327-0926)
14 days70°F (21°C)
MAPEI Kerabond T / Keralastic System
Two-part tile mortar system
21 days73°F (23°C), 50% RH

How to use this table

Open the exact product page to see the variant, source wording, stated conditions and other milestones. A minimum time is the earliest stated threshold under the manufacturer’s conditions—not a guarantee for colder, wetter, thicker or poorly ventilated applications.

Related checks

  • Confirm the exact formula and region on your container.
  • Use the clock for your next action rather than touch-dry time.
  • Check temperature, humidity, thickness and substrate notes.
  • When the manufacturer provides no correction factor, wait longer and verify physical readiness.