Carboguard 890
Epoxy coating with temperature-banded recoat and cure table · US · manufacturer-sourced
How long before you can recoat Carboline Carboguard 890?
Short answer
Film-build schedule
Recoat has a floor and a ceiling, and film thickness moves both
- Prepare the surface and apply the Epoxy coating with temperature-banded recoat and cure table to the stated thickness
- Recoat inside the window the data sheet gives
- Return to service only at the stated cure
This product’s stated stages Quoted at 75°F
- Ready for another coat4 hours
- Full cure1 day
- Immersion-ready5 days
- Recoat window closes30 days
Worth noticing: Recoat inside the window: not before 4 hours and not after 30 days.
Common mistake: Recoating after the maximum window has closed; the next coat may not bond without abrading.
Coat timeline
Plan the next coat and final use separately
- 1ApplyUse the Epoxy coating with temperature-banded recoat and cure table directions and prepare for steel coating and immersion service.
- 2Next coatUse the listed recoat milestone; do not substitute touch-dry time.
- 3Normal useWait for the applicable handling, water or cure milestone.
Check the recoat window
Your countdown
Stated times
- Recoat window closes30 days
- Ready for another coat4 hours
- Immersion-ready5 days
- Full cure1 day
From Carboline data sheet · checked 2026-10-25. Anything not listed isn’t stated by the manufacturer.
Manufacturer website: carboline.com
Conditions & fine print
- Stated conditions: 75°F (24°C)
- Protective-coating times are for the stated film thickness, temperature and humidity. Cold steel, thick films and poor airflow lengthen them. Follow the current data sheet.
- Apply at 50°F or above
- Region US. Formulas can differ between countries; check your container.
- Recoat window closes: It is 90 days over polyurethane.
- Ready for another coat: It is 12 hours at 50°F, 8 hours at 61°F and 2 hours at 90°F.
- Immersion-ready: It is not recommended at 50°F, 10 days at 61°F and 3 days at 90°F.
- Full cure: It is 3 days at 50°F, 2 days at 61°F and 16 hours at 90°F.
- Entered from the cited manufacturer documentation. Check the current label for the exact formula and region. Report outdated information
- Actual results depend on preparation, thickness, ventilation, temperature, humidity, mixing and substrate.
Confirm this is your product
Closely named formulas, colors and regional versions can use different times. Match these details to your container before starting a countdown.
- Exact listing
- Carboline Carboguard 890
- Variant
- Epoxy coating with temperature-banded recoat and cure table
- Region
- US
- Listed use
- steel coating, immersion service
- Timed stages recorded
- recoat max, recoat min, immersion, full cure
- Source checked
- 2026-10-25
Documentation: Technical data sheet · Product data sheet, Jan 2019
Condition attached to the stated time: It is 90 days over polyurethane.
About this product
An epoxy whose data sheet runs on a temperature ladder: recoat falls from 12 hours at 50°F to 2 hours at 90°F, and immersion service is barred entirely at 50°F. Pot life is 3 hours at 25°C.
Using this specific product
Carboline Carboguard 890 is listed here as the Epoxy coating with temperature-banded recoat and cure table version for steel coating and immersion service. For coating steel or industrial surfaces, the useful question is not simply whether the surface looks finished—it is whether the exact next-action milestone shown above has been reached.
Before you start
- Confirm the package says Epoxy coating with temperature-banded recoat and cure table; related versions can use different timing.
- For steel coating and immersion service, pay particular attention to surface preparation, film thickness, temperature, dew point and pot life.
- It is 90 days over polyurethane. It is 12 hours at 50°F, 8 hours at 61°F and 2 hours at 90°F. It is not recommended at 50°F, 10 days at 61°F and 3 days at 90°F. It is 3 days at 50°F, 2 days at 61°F and 16 hours at 90°F.
How to check readiness
Check dry film thickness and the recoat window before the next coat. The sheet gives a maximum recoat window of 30 days over epoxy. Before recoating, confirm the first coat matches the manufacturer’s stated condition; if the maximum window passed, check whether sanding is required. Continuous immersion is more demanding than splashes; wait for the specific immersion milestone.
Avoid this mistake
Recoat windows can close; past the maximum, abrading is usually required.
Compare with similar products
- Compare with Cortec VpCI-396 ConductiveRecoat: 4 h there, 4 h here.
- Compare with Sherwin-Williams Macropoxy EG-1 VHS NRecoat: 4 h there, 4 h here.
Questions
How long before you can recoat this product?
Carboline states: The sheet gives a maximum recoat window of 30 days over epoxy. Conditions: It is 90 days over polyurethane.. The sheet gives recoating with itself after 4 hours at 75°F and 50% humidity. Conditions: It is 12 hours at 50°F, 8 hours at 61°F and 2 hours at 90°F.. The sheet gives immersion service after 5 days at 75°F. Conditions: It is not recommended at 50°F, 10 days at 61°F and 3 days at 90°F.. The sheet gives a general final cure of 1 day at 75°F. Conditions: It is 3 days at 50°F, 2 days at 61°F and 16 hours at 90°F.. These are the manufacturer’s stated times, not a guarantee.
Can Carboguard 890 go into immersion service at 50°F?
No. The sheet marks immersion as not recommended at 50°F and gives 10 days at 61°F, 5 days at 75°F and 3 days at 90°F.
How long does this product take to fully cure?
Carboline states: The sheet gives a general final cure of 1 day at 75°F. Conditions: It is 3 days at 50°F, 2 days at 61°F and 16 hours at 90°F.. These are the manufacturer’s stated times, not a guarantee.
How long before this product can be immersed in water?
Carboline states: The sheet gives immersion service after 5 days at 75°F. Conditions: It is not recommended at 50°F, 10 days at 61°F and 3 days at 90°F.. These are the manufacturer’s stated times, not a guarantee.
What affects how long this product takes to dry or cure?
Protective-coating times are for the stated film thickness, temperature and humidity. Cold steel, thick films and poor airflow lengthen them. Follow the current data sheet. Follow the product label for your conditions.
Similar products
- Carboline Carbomastic 242Aluminum-pigmented mastic, 5 mil dry film · Industrial protective coatings · USRecoat 4 hours
- Carboline Carbomastic 15Aluminum epoxy mastic, 5 to 7 mil · Industrial protective coatings · USRecoat 1 day
- WEG W-DeckDeck coating, three-temperature table · Industrial protective coatings · INTLRecoat 12 hours